J Appl Oral Sci ; 32: e20230458, 2024.
Artículo en Inglés | MEDLINE | ID: mdl-38922241

RESUMEN

OBJECTIVE: This study compared three protocols for developing artificial white spot lesions (WSL) using biofilm models. METHODOLOGY: In total, 45 human enamel specimens were sterilized and allocated into three groups based on the biofilm model: Streptococcus sobrinus and Lactobacillus casei (Ss+Lc), Streptococcus sobrinus (Ss), or Streptococcus mutans (Sm). Specimens were incubated in filter-sterilized human saliva to form the acquired pellicle and then subjected to the biofilm challenge consisting of three days of incubation with bacteria (for demineralization) and one day of remineralization, which was performed once for Ss+Lc (four days total), four times for Ss (16 days total), and three times for Sm (12 days total). After WSL creation, the lesion fluorescence, depth, and chemical composition were assessed using Quantitative Light-induced Fluorescence (QLF), Polarized Light Microscopy (PLM), and Raman Spectroscopy, respectively. Statistical analysis consisted of two-way ANOVA followed by Tukey's post hoc test (α=0.05). WSL created using the Ss+Lc protocol presented statistically significant higher fluorescence loss (ΔF) and integrated fluorescence (ΔQ) in comparison to the other two protocols (p<0.001). RESULTS: In addition, Ss+Lc resulted in significantly deeper WSL (137.5 µm), followed by Ss (84.1 µm) and Sm (54.9 µm) (p<0.001). While high mineral content was observed in sound enamel surrounding the WSL, lesions created with the Ss+Lc protocol showed the highest demineralization level and changes in the mineral content among the three protocols. CONCLUSION: The biofilm model using S. sobrinus and L. casei for four days was the most appropriate and simplified protocol for developing artificial active WSL with lower fluorescence, higher demineralization, and greater depth.


Asunto(s)
Biopelículas , Caries Dental , Esmalte Dental , Lacticaseibacillus casei , Streptococcus mutans , Humanos , Streptococcus mutans/fisiología , Caries Dental/microbiología , Caries Dental/terapia , Esmalte Dental/microbiología , Esmalte Dental/química , Lacticaseibacillus casei/fisiología , Factores de Tiempo , Reproducibilidad de los Resultados , Streptococcus sobrinus/fisiología , Espectrometría Raman , Análisis de Varianza , Microscopía de Polarización , Estadísticas no Paramétricas , Remineralización Dental/métodos , Valores de Referencia , Saliva/microbiología , Saliva/química , Desmineralización Dental/microbiología , Fluorescencia
2.
J. appl. oral sci ; J. appl. oral sci;32: e20230458, 2024. tab, graf
Artículo en Inglés | LILACS-Express | LILACS | ID: biblio-1564708

RESUMEN

Abstract Creating artificial caries-like lesions that mimic the complex changes observed in natural caries is essential for properly evaluating new strategies, dental materials, and devices designed to arrest their progression and avoid more costly and invasive treatments. Objective This study compared three protocols for developing artificial white spot lesions (WSL) using biofilm models. Methodology In total, 45 human enamel specimens were sterilized and allocated into three groups based on the biofilm model: Streptococcus sobrinus and Lactobacillus casei (Ss+Lc), Streptococcus sobrinus (Ss), or Streptococcus mutans (Sm). Specimens were incubated in filter-sterilized human saliva to form the acquired pellicle and then subjected to the biofilm challenge consisting of three days of incubation with bacteria (for demineralization) and one day of remineralization, which was performed once for Ss+Lc (four days total), four times for Ss (16 days total), and three times for Sm (12 days total). After WSL creation, the lesion fluorescence, depth, and chemical composition were assessed using Quantitative Light-induced Fluorescence (QLF), Polarized Light Microscopy (PLM), and Raman Spectroscopy, respectively. Statistical analysis consisted of two-way ANOVA followed by Tukey's post hoc test (α=0.05). WSL created using the Ss+Lc protocol presented statistically significant higher fluorescence loss (ΔF) and integrated fluorescence (ΔQ) in comparison to the other two protocols (p<0.001). Results In addition, Ss+Lc resulted in significantly deeper WSL (137.5 µm), followed by Ss (84.1 µm) and Sm (54.9 µm) (p<0.001). While high mineral content was observed in sound enamel surrounding the WSL, lesions created with the Ss+Lc protocol showed the highest demineralization level and changes in the mineral content among the three protocols. Conclusion The biofilm model using S. sobrinus and L. casei for four days was the most appropriate and simplified protocol for developing artificial active WSL with lower fluorescence, higher demineralization, and greater depth.

3.
J Appl Oral Sci ; 28: e20190737, 2020.
Artículo en Inglés | MEDLINE | ID: mdl-32609185

RESUMEN

OBJECTIVE: Laboratory tests are routinely used to test bonding properties of dental adhesives. Various aging methods that simulate the oral environment are used to complement these tests for assessment of adhesive bond durability. However, most of these methods challenge hydrolytic and mechanical stability of the adhesive- enamel/dentin interface, and not the biostability of dental adhesives. To compare resin-dentin microtensile bond strength (µTBS) after a 15-day Streptococcus mutans (SM) or Streptococcus sobrinus (SS) bacterial exposure to the 6-month water storage (WS) ISO 11405 type 3 test. METHODOLOGY: A total of 31 molars were flattened and their exposed dentin was restored with Optibond-FL adhesive system and Z-100 dental composite. Each restored molar was sectioned and trimmed into four dumbbell-shaped specimens, and randomly distributed based on the following aging conditions: A) 6 months of WS (n=31), B) 5.5 months of WS + 15 days of a SM-biofilm challenge (n=31), C) 15 days of a SM-biofilm challenge (n=31) and D) 15 days of a SS-biofilm challenge (n=31). µTBS were determined and the failure modes were classified using light microscopy. RESULTS: Statistical analyses showed that each type of aging condition affected µTBS (p<0.0001). For Group A (49.7±15.5MPa), the mean µTBS was significantly greater than in Groups B (19.3±6.3MPa), C (19.9±5.9MPa) and D (23.6±7.9MPa). For Group D, the mean µTBS was also significantly greater than for Groups B and C, but no difference was observed between Groups B and C. CONCLUSION: A Streptococcus mutans- or Streptococcus sobrinus-based biofilm challenge for 15 days resulted in a significantly lower µTBS than did the ISO 11405 recommended 6 months of water storage. This type of biofilm-based aging model seems to be a practical method for testing biostability of resin-dentin bonding.


Asunto(s)
Recubrimiento Dental Adhesivo , Recubrimientos Dentinarios , Biopelículas , Resinas Compuestas , Cementos Dentales , Dentina , Ensayo de Materiales , Cementos de Resina , Resistencia a la Tracción
4.
J. appl. oral sci ; J. appl. oral sci;28: e20190737, 2020. tab, graf
Artículo en Inglés | LILACS, BBO - Odontología | ID: biblio-1134793

RESUMEN

Abstract Laboratory tests are routinely used to test bonding properties of dental adhesives. Various aging methods that simulate the oral environment are used to complement these tests for assessment of adhesive bond durability. However, most of these methods challenge hydrolytic and mechanical stability of the adhesive- enamel/dentin interface, and not the biostability of dental adhesives. Objective To compare resin-dentin microtensile bond strength (μTBS) after a 15-day Streptococcus mutans (SM) or Streptococcus sobrinus (SS) bacterial exposure to the 6-month water storage (WS) ISO 11405 type 3 test. Methodology A total of 31 molars were flattened and their exposed dentin was restored with Optibond-FL adhesive system and Z-100 dental composite. Each restored molar was sectioned and trimmed into four dumbbell-shaped specimens, and randomly distributed based on the following aging conditions: A) 6 months of WS (n=31), B) 5.5 months of WS + 15 days of a SM-biofilm challenge (n=31), C) 15 days of a SM-biofilm challenge (n=31) and D) 15 days of a SS-biofilm challenge (n=31). μTBS were determined and the failure modes were classified using light microscopy. Results Statistical analyses showed that each type of aging condition affected μTBS (p<0.0001). For Group A (49.7±15.5MPa), the mean μTBS was significantly greater than in Groups B (19.3±6.3MPa), C (19.9±5.9MPa) and D (23.6±7.9MPa). For Group D, the mean μTBS was also significantly greater than for Groups B and C, but no difference was observed between Groups B and C. Conclusion A Streptococcus mutans- or Streptococcus sobrinus-based biofilm challenge for 15 days resulted in a significantly lower μTBS than did the ISO 11405 recommended 6 months of water storage. This type of biofilm-based aging model seems to be a practical method for testing biostability of resin-dentin bonding.


Asunto(s)
Recubrimiento Dental Adhesivo , Recubrimientos Dentinarios , Resistencia a la Tracción , Ensayo de Materiales , Resinas Compuestas , Biopelículas , Cementos de Resina , Cementos Dentales , Dentina
SELECCIÓN DE REFERENCIAS
DETALLE DE LA BÚSQUEDA