Reis, Raphael Henrique Morais; Nunes, Larissa Fernandes; da Luz, Fernanda Santos; Candido, Verônica Scarpini; da Silva, Alisson Clay Rios; Monteiro, Sergio Neves.
Afiliação
  • Reis RHM; Department of Materials Science, Military Institute of Engineering-IME, Praça General Tibúrcio 80, Urca, Rio de Janeiro 22290-270, Brazil.
  • Nunes LF; Department of Materials Science, Military Institute of Engineering-IME, Praça General Tibúrcio 80, Urca, Rio de Janeiro 22290-270, Brazil.
  • da Luz FS; Department of Materials Science, Military Institute of Engineering-IME, Praça General Tibúrcio 80, Urca, Rio de Janeiro 22290-270, Brazil.
  • Candido VS; Engineering of Natural Resources of the Amazon Program, Federal University of Pará-UFPA, Rua Augusto Corrêa 01, Belém, Pará 66075-110, Brazil.
  • da Silva ACR; Engineering of Natural Resources of the Amazon Program, Federal University of Pará-UFPA, Rua Augusto Corrêa 01, Belém, Pará 66075-110, Brazil.
  • Monteiro SN; Department of Materials Science, Military Institute of Engineering-IME, Praça General Tibúrcio 80, Urca, Rio de Janeiro 22290-270, Brazil.
Polymers (Basel) ; 13(8)2021 Apr 08.
Article em En | MEDLINE | ID: mdl-33917764
Multilayered armor systems (MAS) with a front ceramic layer backed by a relatively unknown Amazonian guaruman fiber-reinforced (Ischnosiphon koem) epoxy composites, as second layer, were for the first time ballistic tested against the threat of 7.62 mm rifle ammunition. The amount of 30 vol% guaruman fibers was investigated in three distinct configurations: (i) continuous aligned, (ii) 0-90° cross-laid, and (iii) short-cut randomly dispersed. Additionally, single-target ballistic tests were also carried out in the best MAS-performed composite with cross-laid guaruman fibers against .22 caliber ammunition. The results disclosed that all composites as MAS second layer attended the US NIJ standard with corresponding penetration depth of (i) 32.9, (ii) 27.5, and (iii) 29.6 mm smaller than the lethal limit of 44 mm in a clay witness simulating a personal body. However, the continuous aligned guaruman fiber composite lost structural integrity by delamination after the 7.62 projectile impact. By contrast, the composite with cross-laid guaruman fibers kept its integrity for subsequent shootings as recommended by the standard. The single-target tests indicated a relatively higher limit velocity for .22 caliber projectile perforation, 255 m/s, and absorbed energy of 106 J for the cross-laid guaruman fibers, which are superior to corresponding results for other less known natural fiber epoxy composites.