Sodium Thiosulfate for Recovery of Bond Strength to Dentin Treated with Sodium Hypochlorite.
Pimentel Corrêa, Ana Carolina; Cecchin, Doglas; de Almeida, José Flávio Affonso; Gomes, Brenda Paula Figueiredo de Almeida; Zaia, Alexandre Augusto; Ferraz, Caio Cezar Randi.
Afiliação
  • Pimentel Corrêa AC; Department of Restorative Dentistry, Piracicaba Dental School, State University of Campinas, Piracicaba, São Paulo, Brazil.
  • Cecchin D; Department of Restorative Dentistry, Passo Fundo Dental School, University of Passo Fundo, Passo Fundo, Rio Grande do Sul, Brazil.
  • de Almeida JF; Department of Restorative Dentistry, Piracicaba Dental School, State University of Campinas, Piracicaba, São Paulo, Brazil.
  • Gomes BP; Department of Restorative Dentistry, Piracicaba Dental School, State University of Campinas, Piracicaba, São Paulo, Brazil.
  • Zaia AA; Department of Restorative Dentistry, Piracicaba Dental School, State University of Campinas, Piracicaba, São Paulo, Brazil.
  • Ferraz CC; Department of Restorative Dentistry, Piracicaba Dental School, State University of Campinas, Piracicaba, São Paulo, Brazil. Electronic address: crandiferraz@gmail.com.
J Endod ; 42(2): 284-8, 2016 Feb.
Article em En | MEDLINE | ID: mdl-26723482
INTRODUCTION: The aim of this study was to evaluate the efficacy of sodium thiosulfate (Na2S2O3) for restoring adhesion to pulp chamber dentin treated with sodium hypochlorite (NaOCl) and EDTA. METHODS: Sixty-three crowns of bovine incisors were cut to expose the dentin pulp chamber. The specimens were polished and randomly distributed into 9 groups (n = 7) according to the following protocols used: 0.9% sodium chloride for 30 minutes (negative control), 5.25% NaOCl for 30 minutes, 17% EDTA for 3 minutes, and 5.25% NaOCl for 1 minute (positive control). The other groups, after treatments with NaOCl and EDTA, were immersed in 0.5% or 5% Na2S2O3 for 1, 5, and 10 minutes or just immersed in an inert solution for 10 minutes (0.9% sodium chloride). After drying the specimens, Scotchbond Multi-Purpose (3M ESPE, St Paul, MN) was applied to the pulp chamber dentin followed by Filtek Z250 composite (3M ESPE). Six rectangular slabs were obtained from each specimen, and the dentin/resin interface was tested by using a universal testing machine. The resulting data were submitted to 1-way analysis of variance and the Duncan test (P = .05). RESULTS: There was a significant decrease in bond strength regarding NaOCl and EDTA (P < .05). When 5% Na2S2O3 was used for 10 minutes, the bond strength was found to be statistically equal to the negative control and higher than the positive control (P < .05). CONCLUSIONS: The use of Na2S2O3 can significantly increase the bond strength of composite resin to NaOCl/EDTA-treated dentin, allowing adhesive restorations to be immediately applied after endodontic treatment.
Assuntos
Palavras-chave

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Hipoclorito de Sódio / Tiossulfatos / Adesivos Dentinários / Dentina Tipo de estudo: Guideline Limite: Animals Idioma: En Revista: J Endod Ano de publicação: 2016 Tipo de documento: Article País de afiliação: Brasil País de publicação: Estados Unidos

Texto completo: 1 Coleções: 01-internacional Base de dados: MEDLINE Assunto principal: Hipoclorito de Sódio / Tiossulfatos / Adesivos Dentinários / Dentina Tipo de estudo: Guideline Limite: Animals Idioma: En Revista: J Endod Ano de publicação: 2016 Tipo de documento: Article País de afiliação: Brasil País de publicação: Estados Unidos