Effect of superficial treatment on the tensile bond strength of two reliners and a thermopolymerizable resin
Braz. j. oral sci
; 6(20): 1295-1300, Jan-Mar. 2007. ilus, tab
Article
em En
| LILACS, BBO
| ID: biblio-850528
Biblioteca responsável:
BR28.1
Localização: BR28.1; BR97.1
ABSTRACT
The study aims to evaluate the tensile bond strength of two direct hard reliners, Kooliner and Tokuyama Rebase II and a thermopolymerizable acrylic resin, Vipi Cril, following mechanical superficial treatment. Forty specimens were prepared and separated in four groups according to the relining material and the surface treatment of the thermopolymerizable resin group I - Kooliner joined to the surface of the resin without treatment, group II û Kooliner joined to the surface of the resin with treatment, group III û Tokuyama joined to the surface of the resin without treatment and group IV - Tokuyama joined to the surface of the resin with treatment. Obtained values were statistically compared by the Bartlett's test and variance analysis to 5%. The results are presented in Kgf Group 1, 74.35 ± 15.89; Group 2, 104.95 ± 13.97; Group 3, 86.91 ± 14.63; Group 4, 100.42 ± 14.93. No significant difference was found between the reliners. The mechanical superficial treatment on the thermopolymerizable resin for denture base has significantly increased its tensile bond strength with the studied reliners.
Texto completo:
1
Coleções:
01-internacional
Base de dados:
BBO
/
LILACS
Assunto principal:
Resistência à Tração
/
Materiais Dentários
/
Prótese Total
/
Reembasadores de Dentadura
Idioma:
En
Revista:
Braz. j. oral sci
Assunto da revista:
ODONTOLOGIA
Ano de publicação:
2007
Tipo de documento:
Article
País de afiliação:
Brasil
País de publicação:
Brasil