Nonthermal plasma on the shear bond strength of relining resin to thermoplastic denture base resin / 대한치과보철학회지
Article en En | WPRIM | ID: wpr-715998
Biblioteca responsable: WPRO
ABSTRACT
PURPOSE: This study evaluated the effect of nonthermal plasma treatment on the bond strength of autopolymerizing relining resin to the injection molded thermoplastic denture base resins (TDBRs) with different surface treatments. MATERIALS AND METHODS: Acrylic Resin (Acrytone), Polyester (Estheshot-Bright), Polyamide (Valplast) and Polypropylene (Weldenz) were subjected to various surface treatments: No treatment, Nonthermal plasma, Sandblasting, Sandblasting and nonthermal plasma. Specimens were bonded using an autopolymerizing relining resin. Shear bond strength was tested using universal testing machine with crosshead speed of 1 mm/min. Statistical analysis by two-way analysis of variance with Tukey's test post hoc was used. RESULTS: Acrytone showed significantly higher shear bond strength value among other TDBR group while Weldenz had the lowest. The sandblasting and nonthermal plasma condition had significantly higher shear bond strength value in all of the resin groups (P < .05). CONCLUSION: The use of nonthermal plasma treatment showed limited effect on the shear bond strength between TDBRs and relining resin, and combination of nonthermal plasma and sandblasting improved the shear bond strength between TDBR and reline material.
Asunto(s)
Palabras clave
Texto completo: 1 Base de datos: WPRIM Asunto principal: Plasma / Poliésteres / Polipropilenos / Dentaduras / Bases para Dentadura / Hongos / Nylons Idioma: En Revista: The Journal of Korean Academy of Prosthodontics Año: 2018 Tipo del documento: Article
Texto completo: 1 Base de datos: WPRIM Asunto principal: Plasma / Poliésteres / Polipropilenos / Dentaduras / Bases para Dentadura / Hongos / Nylons Idioma: En Revista: The Journal of Korean Academy of Prosthodontics Año: 2018 Tipo del documento: Article