Your browser doesn't support javascript.
loading
The Influence of Laser Process Parameters on the Adhesion Strength between Electroless Copper and Carbon Fiber Composites Determined Using Response Surface Methodology.
Wang, Xizhao; Liu, Jianguo; Liu, Haixing; Zhou, Zhicheng; Qin, Zhongli; Cao, Jiawen.
Afiliación
  • Wang X; Institute of Laser and Intelligent Manufacturing Technology, South-Central Minzu University, Wuhan 430074, China.
  • Liu J; Wuhan National Laboratory for Optoelectronics (WNLO), Huazhong University of Science and Technology (HUST), Wuhan 430074, China.
  • Liu H; Wuhan National Laboratory for Optoelectronics (WNLO), Huazhong University of Science and Technology (HUST), Wuhan 430074, China.
  • Zhou Z; Institute of Laser and Intelligent Manufacturing Technology, South-Central Minzu University, Wuhan 430074, China.
  • Qin Z; Wuhan National Laboratory for Optoelectronics (WNLO), Huazhong University of Science and Technology (HUST), Wuhan 430074, China.
  • Cao J; School of Electronics and Information Engineering, Hubei University of Science and Technology, Xianning 437100, China.
Micromachines (Basel) ; 14(12)2023 Nov 29.
Article en En | MEDLINE | ID: mdl-38138337
ABSTRACT
Laser process technology provides a feasible method for directly manufacturing surface-metallized carbon fiber composites (CFCs); however, the laser's process parameters strongly influence on the adhesion strength between electroless copper and CFCs. Here, a nanosecond ultraviolet laser was used to fabricate electroless copper on the surface of CFCs. In order to achieve good adhesion strength, four key process parameters, namely, the laser power, scanning line interval, scanning speed, and pulse frequency, were optimized experimentally using response surface methodology, and a central composite design was utilized to design the experiments. An analysis of variance was conducted to evaluate the adequacy and significance of the developed regression model. Also, the effect of the process parameters on the adhesion strength was determined. The numerical analysis indicated that the optimized laser power, scanning line interval, scanning speed, and pulse frequency were 5.5 W, 48.2 µm, 834.0 mm/s, and 69.5 kHz, respectively. A validation test confirmed that the predicted results were consistent with the actual values; thus, the developed mathematical model can adequately predict responses within the limits of the laser process parameters being used.