1.
Philos Trans A Math Phys Eng Sci ; 373(2038)2015 Mar 28.
Artículo en Inglés | MEDLINE | ID: mdl-25713455

RESUMEN

Diamond coating of suitable template materials and subsequent delamination allows for the manufacturing of free-standing diamond foil. The evolution of the microstructure can be influenced by secondary nucleation via control of process conditions in the hot-filament chemical vapour deposition process. Bending tests show extraordinarily high strength (more than 8 GPa), especially for diamond foils with nanocrystalline structure. A detailed fractographic analysis is conducted in order to correlate measured strength values with crack-initiating defects. The size of the failure causing flaw can vary from tens of micrometres to tens of nanometres, depending on the diamond foil microstructure as well as the loading conditions.

SELECCIÓN DE REFERENCIAS
DETALLE DE LA BÚSQUEDA